Thermal Paste, Thermal Pads, Phase-Change and Liquid Metal — What’s the Difference?
In every laptop, games console and PC, a thin layer of material sits between the processor and its cooler. It can be thermal paste, a phase-change material such as PTM7950, a thermal pad or liquid metal — four very different materials, each with its own strengths and risks.
This guide explains how each one works, what their makers actually publish — including why their W/mK figures can’t be compared — where device makers use them, and what we use in our own workshop in Limassol. Every factual claim links to its source; where we describe our own practice, we say so.
In short
- All four do the same job: fill the gap between chip and cooler. Even flat-looking metal surfaces have microscopic imperfections, and the air trapped in them acts as a barrier to heat.37,45
- Thermal paste is the classic choice, but it ages. As the chip heats up and cools down, paste can be pumped out of the gap or dry out, and its thermal resistance rises.45,5
- Phase-change materials (PCM) are solid at room temperature and soften once warm — from around 45–50 °C, depending on the product. Their makers say they resist pump-out, but they need enough mounting pressure and a first heat-up to reach full performance.10,11,15,14,17
- Thermal pads fill wider gaps, and thickness is everything. A pad should be slightly thicker than the gap so that it compresses — but a pad that is too thick can hold the cooler away from the main chip.22,28
- Liquid metal is a gallium alloy, and it conducts electricity. A stray drop can short components; gallium attacks aluminium and reacts with copper. Sony, ASUS and Lenovo use it with insulation or barriers around the chip.31,36,39,40,44
- Don’t shop by W/mK. Noctua, Thermal Grizzly and ARCTIC don’t publish thermal conductivity for their pastes, and one Henkel material is rated 5.3 or 8.5 W/mK depending on the test method.1,2,7,19
- From our workshop: when we service the cooling of a laptop or a console, we almost always fit PTM7950 instead of paste — it’s included in our cooling-system cleaning and maintenance, from €80.
Why a thermal interface is needed at all
A processor and the base of its cooler look flat, but they aren’t perfectly so. Intel explains that these metal plates have microscopic imperfections that can result in poor heat transfer, and that thermal paste fills in those air gaps.37 ARCTIC describes the same surfaces as covered with microscopic dents.6 A 2000 paper in the Intel Technology Journal put it in engineering terms: voids at the interface are air gaps that act as barriers to heat conduction.45
The aim is to fill those gaps, not to keep the surfaces apart: Intel warns that too much paste reduces its efficacy, because the metal surfaces end up too far apart.37 Where the gap is wider, pads take over. ARCTIC suggests thermal grease rather than a pad when there is almost no gap (under 0.2 mm),27 and Thermal Grizzly says factory graphics cards typically use thermal pads in two or three different heights.23 One device can combine several materials: Lenovo’s service procedure for the Legion Pro 7 puts liquid metal on the CPU and thermal grease on the GPU.44
Thermal paste
Thermal paste is a carrier filled with fine particles — the Intel paper describes it as a polymer and filler matrix.45 Recipes differ by brand: Noctua describes NT-H2 as a mixture of metal oxide micro-particles; Thermal Grizzly makes Duronaut from silicone oil with aluminium micro-powder and zinc oxide nano-powder; ARCTIC uses carbon microparticles in MX-5 and a silicone gel carrier in MX-6.1,5,6 Unlike liquid metal, the pastes in this guide are described by their makers as not electrically conductive: Noctua, Thermal Grizzly, Gelid and Thermalright say so for their pastes, and ARCTIC for MX-4 and MX-5.1,2,8,9,6
How paste ages: pump-out and dry-out
The same Intel paper described two ways paste fails between a bare chip and a heatsink. In pump-out, relative motion (flexure) between the die and the heatsink base squeezes grease out of the interface. In dry-out, the polymer and the filler separate, and thermal resistance rises.45 Thermal Grizzly defines pump-out as the displacement of paste caused by temperature fluctuations, and says it is particularly critical where different materials meet — such as a silicon chip (for example in a GPU) and a copper heatsink.5
The Intel paper also reported a twofold increase in degradation for every 10 °C rise in average operating temperature. That figure is from 2000, so treat it as an illustration of the trend rather than a rule for today’s pastes.45
Makers tackle ageing in different ways: Thermal Grizzly says Duronaut is formulated to minimise pump-out and doesn’t harden over time; ARCTIC describes MX-6 as non-drying and non-bleeding and lists “No Pump-Out Effect” for MX-7.5,6 As for how often to replace it, Intel says you shouldn’t need to reapply paste more than once every few years — but that you should replace it whenever you remove the cooler for any reason. Noctua gives a recommended usage time of up to 5 years on the CPU for NT-H1 and NT-H2.37,1
What paste makers publish — and what they don’t
You might expect every pack to state a thermal conductivity in W/mK. Many don’t. Noctua’s datasheets for NT-H1 and NT-H2 give none.1 Thermal Grizzly says that since the fourth quarter of 2020 none of its cooling products give specific thermal-conductivity values; it calls such values mostly theoretically determined and says they vary greatly depending on the application, because contact pressure, temperature and surface can’t be taken into account uniformly.2 ARCTIC doesn’t publish them either, saying that many manufacturers invent, artificially inflate or embellish this value.7 Gelid and Thermalright do publish figures. Why those figures can’t be compared is explained below.
Popular paste brands — what their makers say
| Brand and products | What the maker publishes |
|---|---|
| Noctua NT-H1, NT-H2 | No thermal conductivity figure. “Not electrically conductive, non-corroding”. Recommended usage time on the CPU up to 5 years; storage before use up to 3 years. NT-H1: −50 to 110 °C, no break-in or burn-in required. NT-H2: −50 to 200 °C.1 |
| Thermal Grizzly Aeronaut, Kryonaut, Duronaut | No W/mK since the fourth quarter of 2020; regular Thermal Grizzly pastes are not electrically conductive; an opened tube can be used for at least 3 years. Aeronaut: an “ideal entry-level product” for CPUs, GPUs, notebooks and ICs, with no curing. Kryonaut: “designed for Overclocking”; “does not even begin to dry out at 80 °C”. Duronaut: formulated to minimise pump-out, no hardening over time.2,3,4,5 |
| ARCTIC MX-4, MX-5, MX-6, MX-7 | No W/mK, as a matter of policy. MX-4: metal-free and not electrically conductive; continuous use −50 to 150 °C. MX-5: “neither electrically conductive nor capacitive”. MX-6: non-drying and non-bleeding. MX-7: “No Pump-Out Effect”; suitable for CPUs, GPUs, laptops and console processors; −50 to 250 °C.6,7 |
| Gelid GC-Extreme | Thermal conductivity 8.5 W/mK (maker’s figure). Non-electrically conductive; non-corrosive, non-curing and non-toxic; no bleeding. −45 to +180 °C.8 |
| Thermalright TF7, TF8 | 12.8 and 13.8 W/m-K (maker’s figures); thermal impedance under 0.01 °C·cm²/W; electrically conductive: no.9 |
Brands are listed for information, not ranked. Every figure is the maker’s own — don’t compare them across brands (here’s why).
Phase-change materials (PCM)
A phase-change thermal interface material is solid at room temperature and softens when heated. Solstice, which now makes PTM7950, says this lets it fully fill the gaps between the contact surfaces, giving a thin bondline and high reliability without pump-out issues.10 Henkel describes the same effect for its Hi-Flow material: it flows at its phase-change temperature, conforms to the surface features of the components, and air is expelled from the interface.19
Despite the name, most modern PCMs don’t actually melt. Laird explains that the first PCMs melted to a liquid at 50–60 °C, while today most of them soften at operating temperatures in the 50–70 °C range instead — which makes them much more resistant to pump-out.13 The exact temperature depends on the product: Thermal Grizzly says PhaseSheet PTM only begins to liquefy above 45 °C; Laird gives about 45 °C for Tpcm 780 and about 50 °C for Tpcm 7000; Henkel lists 45 °C for Hi-Flow THF 5000UT; and Solstice’s selection guide lists 45 °C as a common property of its PCM range.17,15,14,19,12
What a PCM needs: pressure and a first heat-up
A PCM needs two things to work properly. The first is clamping force: Solstice says PTM7950 needs 30–40 psi in use, Thermal Grizzly asks for a high contact pressure of around 300–400 N for PhaseSheet PTM, and Laird notes that PCMs are generally used under constant pressure, with some type of spring-loaded heatsink.11,17,13 The second is heat: Solstice says the material must go through its phase-change temperature to reach its full rated performance; Laird’s instructions for Tpcm 7000 call for more than 60 °C at the heatsink for more than 3 minutes at over 25 psi; and Thermal Grizzly says PhaseSheet PTM develops and stabilises its maximum thermal conductivity after around ten thermal cycles above 60 °C.11,16,17
After that, it stays where it is. Laird says that once the material has “wetted” the surface it cannot be repositioned; to rework, the parts are warmed to over 40 °C to separate them, the old material is cleaned off and new material is applied.16 So, as with paste, a PCM is replaced whenever the cooler comes off.37,16
Popular PCM products
| Product | What the maker publishes |
|---|---|
| Solstice (formerly Honeywell) PTM7950 | Now sold by Solstice Advanced Materials, created through the 2025 spin-off of Honeywell’s former Advanced Materials business. Thermal conductivity 8.5 W/m-K (ASTM D5470). “Silicone-free, no pump out, bleed out, dry out issues”; “long service life under thermal cycling”. In Solstice’s tests, thermal impedance was 0.04 °C·cm²/W after 1,000 hours of baking at 150 °C, and 0.045 after 1,000 temperature cycles from −55 to +125 °C. Supplied as pads in sheets and rolls, and in paste versions (PTM7950-SPS, PTM7950-SP); listed uses include CPUs and GPUs in networks, notebooks, PCs and tablets. Shelf life 12 months.11 |
| Laird Tpcm 7000, Tpcm 780 | Tpcm 7000: 7.5 W/m-K (Hot Disk method); softens at about 50 °C, when the pad can thin to a bondline as thin as 25 µm; “No pump out”; markets include graphics cards and game consoles.14 Tpcm 780: 5.4 W/m-K; begins to soften and flow at about 45 °C; a polymer matrix that doesn’t fully change phase, which Laird says drastically minimises pump-out; easy to rework; markets include notebooks.15 |
| Thermal Grizzly PhaseSheet PTM | A pad that is solid at room temperature and liquefies in operation, above 45 °C. Electrically non-conductive; −75 to 150 °C; needs around 300–400 N. Contracts again when it turns solid, which minimises pump-out. “More durable than traditional thermal pastes, but not as durable as KryoSheet”; “virtually maintenance-free”. No W/mK published.17 |
| Henkel Bergquist Hi-Flow THF 5000UT | Phase-change temperature 45 °C; operating temperature −40 to 150 °C. Thermal conductivity 5.3 W/mK (ASTM D5470, multiple thicknesses) or 8.5 W/mK (modified ASTM D5470 for thin-bondline materials) — for the same material. Easy to handle and rework.19 |
| Shin-Etsu PCS-LT-30 | Softens and flows at elevated temperature to fill the voids, with thermal performance Shin-Etsu describes as “almost as high as Thermal Grease”. 3.00 W/m·K; softening point given as 50; “Excellent pump-out resistance”. Typical applications: CPUs, GPUs, power supplies and IGBTs.20 |
Listed for information, not ranked. The W/mK figures were measured by different methods and can’t be compared (here’s why).
Device makers fit PCMs at the factory too. ASUS uses a phase-change GPU thermal pad on graphics cards such as the ROG Astral RTX 5080, without naming the supplier, and MSI says its laptops use its own proprietary phase-change thermal pads.42,43
Don’t confuse it with KryoSheet. Thermal Grizzly’s KryoSheet is a graphene thermal sheet, not a phase-change material — and unlike PhaseSheet PTM it is electrically conductive. Thermal Grizzly doesn’t recommend using a KryoSheet more than once.18
Thermal pads and putty
Thermal pads are soft sheets that fill gaps too wide for paste. ARCTIC suggests thermal grease instead of a pad when there is almost no gap (under 0.2 mm), and says a gap of more than 3 mm is a reason to review the design, because pads are meant for small gaps.27 ARCTIC also notes that pads don’t conduct heat quite as well as pastes, but can be cut to size and shape, which makes them easier to use, especially for beginners.29 Factory graphics-card coolers typically use pads in two or three different heights, according to Thermal Grizzly.23
Thickness: the rule that matters most
A pad only works when it is pressed between the component and the cooler. ARCTIC recommends a pad thick enough to get between 10% and 40% compression — for example, a 1.0 mm pad to bridge a 0.7 mm gap.28 Gelid says its GP-Extreme and GP-Ultimate pads can be compressed by up to 30% of their thickness with adequate mounting pressure.24 When replacing pads, ARCTIC advises checking that the new pad is the same thickness as the one you are replacing — and, on a graphics card with no published information, measuring the old pad.27
Too thick is a problem too. Thermal Grizzly says its High Compression pads should be slightly thicker than the measured height difference, but warns against pads that are too thick: direct contact between the GPU chip and its cooler must always be maintained. In other words, a pad that is too thick can hold the cooler off the main chip.22 Gelid recommends the thinnest possible pad for efficient heat transfer.24 And thickness costs performance even when the fit is right: in Fujipoly’s data for SARCON GR130A at 100 kPa, thermal resistance rises from 0.3 K·cm²/W at 0.3 mm to 0.7 at 1.0 mm and 1.3 at 2.0 mm.25
Stacking and reuse: makers disagree
Gelid says it’s not recommended to stack one pad on top of another. ARCTIC, by contrast, says its soft TP-3 pads can be stacked particularly well, while harder pads often lose performance when stacked.24,26 On reuse, Gelid says thermal pads cannot be reused, Thermal Grizzly recommends only one-time use for Minus Pad Extreme, and ARCTIC says a TP-3 pad can be reused as long as it doesn’t look degraded — hardened, dirty or oily.24,21,27 Pads also change with age: in Fujipoly’s test, SARCON GR130A hardened from 74 to 94 Shore OO after 1,000 hours at 150 °C.25
Thermal putty
Thermal putty is an alternative to pads. Thermal Grizzly says TG Putty can bridge height differences from 0.2 to 3.0 mm and is electrically non-conductive — but is not suitable for processors or for use directly on a GPU die.23
Popular pad brands
| Brand and products | What the maker publishes |
|---|---|
| Thermal Grizzly Minus Pad Extreme 2, Minus Pad High Compression, TG Putty | No W/mK in the current datasheets. Minus Pad Extreme 2: “Electrically non-conductive”. High Compression: meant for situations where the exact required thickness is unknown, and chosen slightly thicker than the measured gap. TG Putty: 0.2–3.0 mm, −40 to +120 °C, not for processors or GPU dies.21,22,23 |
| Gelid GP-Extreme, GP-Ultimate | Gelid’s FAQ: “We don’t use the W/mK rating since it may vary depending on your application and doesn’t reflect real-world performance” — although GP-Ultimate was launched with a 15 W/mK claim. Not electrically conductive; compressible by up to 30%; GP-Ultimate −60 to 220 °C; not reusable; stacking not recommended.24 |
| Fujipoly SARCON GR130A | 13.0 W/m-K (ISO 22007-2, Hot Disk); 0.3–2.0 mm; −40 to +150 °C; breakdown voltage 14 kV/mm; thermal resistance rises with thickness; hardens with heat ageing.25 |
| ARCTIC TP-3 | No W/mK, as a matter of policy. 55 Shore OO; compression ratio 42% at 50 psi; −40 to 150 °C; “electrically insulating, non-adhesive, and easy to handle”; 0.5, 1 and 1.5 mm.26,7 |
| Thermalright Odyssey, Odyssey II | 12.8 and 14.8 W/mK (maker’s figures); electrically conductive: no. No temperature range or compression figures published.30 |
Listed for information, not ranked; figures are the makers’ own.
Liquid metal
Liquid-metal thermal compounds are gallium-based alloys that stay liquid in use. Thermal Grizzly’s Conductonaut is 60–70% gallium, 10–20% indium and 10–20% tin, and is applied at 8–150 °C; Conductonaut Extreme contains only gallium and indium.32,31,34 Indium Corporation’s industrial alloys 51E and 300E melt at 11 °C and 15.7 °C.36
Their appeal is heat transfer. Thermal Grizzly calls Conductonaut’s thermal conductivity “ultra high” without giving a figure, and says Conductonaut Extreme conducts about 18% more; Thermalright states 79 W/m-K for Silver King.31,34,35 ASUS says liquid metal conducts 17 times more heat than paste, and that in its laptops it lowers temperatures by about 10 °C on average.41
The risks: electricity, aluminium and copper
- It conducts electricity. Thermal Grizzly lists Conductonaut as not electrically insulating, and Thermalright states that Silver King is electrically conductive.31,35 Intel warns that if liquid metal touches the capacitors on a processor package, it can cause immediate failure, or degradation and instability later.38 Indium Corporation says it must not touch circuitry.36
- It destroys aluminium. Thermal Grizzly says Conductonaut must not be used with aluminium coolers, and that contact permanently damages the cooling unit. Indium says aluminium — anodised or not — is not acceptable, and warns of possible sudden catastrophic failure shortly after contact.31,33,36 Research explains why: liquid gallium penetrates aluminium’s grain boundaries, so the metal fractures mostly between the grains even with no applied stress; in a 2025 study, aluminium’s fracture elongation fell by 60% after contact with liquid gallium at 80 °C for 40 minutes.46,47
- It reacts with copper. Gallium forms intermetallic compounds with copper — mainly CuGa₂ and Cu₉Ga₄ at low temperatures. CuGa₂ is brittle, and as these compounds grow, the copper surface is consumed.48 Indium Corporation says gallium diffuses into copper heatspreaders and heatsinks and, under varying temperatures, this could lead to early failure.36 In a Purdue University study of gallium-indium alloy between nickel-plated copper, these reactions used up gallium at elevated temperature and left an indium-rich alloy.50
- Nickel plating helps, but isn’t permanent. Thermal Grizzly and Thermalright recommend nickel-plated surfaces, and Indium recommends electroless nickel plating of 20 nm or more on copper.31,35,36 In lab tests at 160–280 °C, a nickel layer worked as a diffusion barrier but was gradually consumed, after which copper-gallium compounds formed underneath.49
- It can leave marks. Thermal Grizzly notes that Conductonaut may leave optical residues, and that if it diffuses into a heatspreader the engraving can become illegible and the warranty may be voided. Intel says liquid metal can be corrosive, may erase CPU markings and can void a boxed processor’s warranty.31,38
How device makers use it
The companies that put liquid metal into their products surround it with protection.
- Sony PlayStation 5. Sony says all PS5 consoles use liquid metal on the main processor. Its PS5 Pro mechanical design lead calls using it in the original PS5 “challenging”: it was adopted after various safety tests and long research into insulation, and the PS5 Pro keeps the same structure but adds fine grooves where the liquid metal is applied, for more stable cooling. Sony also warns owners not to take the console apart at home — doing so voids the guarantee.39
- ASUS ROG laptops. ASUS first used liquid metal in the ROG Mothership in 2019 and then across its 2020 ROG lineup with 10th-gen Intel processors, choosing Thermal Grizzly Conductonaut for its lower tin content. A special sponge around the die fills a 0.1 mm gap to stop the metal seeping out and causing shorts. ASUS explains that Intel CPUs have a capacitor-free zone around the die, while other processors have components there that are prone to shorting. Top ROG laptops have used Conductonaut Extreme since 2022.40,41,34
- Lenovo Legion Pro 7. Lenovo’s service procedure for the Intel Legion Pro 7 applies about 0.2 g of liquid metal to the CPU only, with thermal grease on the GPU. It requires a protective sheet because spills onto components cause short circuits, tells technicians not to remove the CPU’s conformal coating, and replaces the sponge fence around the chip if it is deformed or stained.44
Liquid-metal brands we could verify
We could verify liquid-metal products on their makers’ own pages for only three companies: Thermal Grizzly, Thermalright and Indium Corporation. We don’t list others.
| Brand and product | What the maker publishes |
|---|---|
| Thermal Grizzly Conductonaut | Gallium, indium and tin; 6.24 g/cm³; application 8–150 °C, operation −50 to +200 °C. Electrically conductive; not for aluminium coolers; nickel-plated surfaces recommended. No W/mK figure published by Thermal Grizzly.31,32 |
| Thermal Grizzly Conductonaut Extreme | Gallium and indium only, formulated so that interactions with tin can’t occur; about 18% more thermal conductivity than Conductonaut (no absolute figure); 6.29 g/cm³; application 17–150 °C. Electrically conductive; nickel-plated copper recommended, not for aluminium. Used by ASUS in top ROG laptops since 2022.34 |
| Thermalright Silver King | 79 W/m-K (maker’s figure). A 100% liquid-metal alloy without non-metallic additives; the elements aren’t disclosed. Electrically conductive; not for aluminium; recommended for nickel-plated copper.35 |
| Indium Corporation (industrial) | Gallium alloys such as 51E (66.5% gallium, 20.5% indium, 13% tin; melts at 11 °C) and 300E (78.6% gallium, 21.4% indium; 15.7 °C). Indium calls its alloy 306 an industry standard in HPC, AI-server and high-end gaming platforms. Its own documents give different W/mK values for the same 300E alloy — 44 at 85 °C in one, an estimated 21 in another. Recommends 15–20 mg for a 25.4 × 25.4 mm die.36 |
From our workshop: we apply liquid metal only when a customer asks for it, with protection of the surrounding components. Customers often bring us devices in which liquid metal had been mixed with thermal paste, and we see black stains on chips and heatsinks where the liquid metal was missing or had dried out. We found no manufacturer guidance on mixing the two; Thermal Grizzly’s application guide simply says both surfaces must be clean, dry and free of residue before liquid metal goes on.33 We’ll cover liquid-metal damage in a separate guide.
Side by side — and why W/mK can’t be compared
A summary of what the makers and studies cited in this guide say. “Not published” means none of our sources gives it.
| Thermal paste | Phase-change (PCM) | Pads and putty | Liquid metal | |
|---|---|---|---|---|
| What it’s for | The thin layer between chip and cooler; for gaps under 0.2 mm, ARCTIC suggests grease rather than a pad.37,27 | The same place as paste — CPUs and GPUs.11,20 | Wider gaps: from about 0.2 mm up to 3 mm per ARCTIC; TG Putty 0.2–3.0 mm.27,23 | Directly on the die or on a nickel-plated heatspreader; Lenovo uses it on the CPU only.33,44 |
| Form | A carrier filled with fine particles.45,5 | Solid at room temperature, softens when warm; sheets, rolls or paste versions.10,11 | Soft sheets cut to size; putty for height differences.29,23 | A liquid gallium alloy.32 |
| Conducts electricity? | No, according to Noctua, Thermal Grizzly, ARCTIC (MX-4, MX-5), Gelid and Thermalright.1,2,6,8,9 | Thermal Grizzly: PhaseSheet PTM is non-conductive. Solstice publishes a volume resistivity for PTM7950 rather than a plain “non-conductive”.17,11 | No, according to Gelid, Thermal Grizzly, ARCTIC and Thermalright.24,21,26,30 | Yes.31,35,38 |
| Main risks | Pump-out and dry-out over time; too much paste works worse.45,37 | Needs enough pressure and a first heat-up; can’t be repositioned once it has wetted the surface.11,16 | Wrong thickness: too thick can keep the cooler off the main chip; thicker pads have higher thermal resistance.22,25 | Short circuits; destroys aluminium; reacts with copper; can leave marks.38,36,48,31 |
| Service life — what makers say | Noctua: up to 5 years on the CPU. Intel: every few years, and whenever the cooler is removed.1,37 | Solstice: no pump-out, bleed-out or dry-out issues; long service life under thermal cycling. Thermal Grizzly: virtually maintenance-free.11,17 | Not published. Makers disagree about reuse.24,27 | Not published. Gallium keeps reacting with copper, and even with nickel barriers (lab studies).48,49 |
| Factory use — examples | Lenovo Legion Pro 7 GPU.44 | ASUS graphics cards; MSI laptops.42,43 | Graphics-card coolers, in two or three heights.23 | All PS5 consoles; ASUS ROG laptops since 2019; Lenovo Legion Pro 7 CPU.39,40,44 |
On a phone, swipe the table sideways.
Why we don’t rank anything by W/mK
- The test method changes the number. Henkel rates the same Hi-Flow THF 5000UT at 5.3 W/mK by one ASTM D5470 method and 8.5 W/mK by a modified version for thin bondlines.19 Across brands the methods differ too: Solstice uses ASTM D5470 for PTM7950, Laird the Hot Disk method for Tpcm 7000, and Fujipoly ISO 22007-2 for SARCON GR130A.11,14,25
- Even one maker’s figures don’t agree. For its 300E alloy, Indium Corporation gives 44 W/mK (at 85 °C) in one document and an estimated 21 in another.36
- Real conditions matter more. Thermal Grizzly says W/mK values vary greatly with contact pressure, temperature and surface; Gelid says the rating doesn’t reflect real-world performance; ARCTIC says the minimum layer thickness is just as important as the conductivity value.2,24,6
- Many makers don’t publish it at all — among them Noctua, Thermal Grizzly and ARCTIC.1,2,7
That’s why the figures in this guide are quoted exactly as each maker publishes them, with the test method where one is given — and never as a ranking.
What we use in our workshop — and why
From our workshop — this is our own practice, not a manufacturer’s recommendation:
- PTM7950 instead of paste. When we service the cooling of a laptop or a games console, we almost always fit Honeywell PTM7950 phase-change material — now made by Solstice, Honeywell’s 2025 spin-off — instead of thermal paste. Why: paste ages through pump-out and dry-out, while Solstice states that PTM7950 has no pump-out, bleed-out or dry-out issues.45,11
- When we do use paste, it’s Noctua or Thermal Grizzly Aeronaut. We don’t use ARCTIC MX-4, MX-5 or MX-6, or cheap pastes.
- Liquid metal on request. We apply it when a customer asks for it, with protection of the surrounding components.
- Price: cleaning and maintenance of the cooling system is from €80, and replacing the paste with PTM7950 is included in that price.
- Diagnostics: €40, and you get a fixed quote before any work begins.
- Getting it to us: walk in to our Limassol workshop; laptops can also come by ACS courier from anywhere in Cyprus — return shipping is on us.
FAQ
Is PTM7950 better than thermal paste?
How often should thermal paste be replaced?
Which thermal paste has the highest W/mK?
Is thermal paste electrically conductive?
Is liquid metal safe in a laptop or console?
Can I use liquid metal with an aluminium heatsink?
Can thermal pads be reused, and what thickness do I need?
How much does a cooling service cost at your workshop?
Sources
All sources are in English. All links checked on 8 October 2026.
Thermal paste
- Noctua — NT-H1 3.5g datasheet · NT-H2 3.5g datasheet
- Thermal Grizzly — FAQ
- Thermal Grizzly — Aeronaut · Aeronaut datasheet
- Thermal Grizzly — Kryonaut · Kryonaut datasheet
- Thermal Grizzly — Duronaut · Duronaut datasheet
- ARCTIC — MX-4 · MX-5 · MX-6 · MX-7 (product pages)
- ARCTIC — FAQ: Why doesn’t ARCTIC communicate thermal conductivity values? (US version)
- Gelid — GC-Extreme · GC-Extreme 3.5g specification
- Thermalright — TF7 · TF8 thermal paste (product pages)
Phase-change materials
- Solstice Advanced Materials — Phase Change Materials
- Solstice Advanced Materials — PTM7950 · PTM7950 technical data sheet (August 2026)
- Solstice Advanced Materials — Choose your phase change material (selection guide, 07/26)
- Laird — Phase Change Materials
- Laird — Tpcm 7000 data sheet
- Laird — Tpcm 780 data sheet
- Laird — Tpcm 5000, Tpcm 7000, Tpcm 7000Plus — Instructions for Use
- Thermal Grizzly — PhaseSheet PTM · PhaseSheet PTM datasheet
- Thermal Grizzly — KryoSheet
- Henkel — BERGQUIST HI FLOW THF 5000UT technical data sheet (April 2024)
- Shin-Etsu Silicones — Phase Change Materials · PCS-LT-30 data sheet
Thermal pads and putty
- Thermal Grizzly — Minus Pad Extreme datasheet · Minus Pad Extreme 2 datasheet
- Thermal Grizzly — Minus Pad High Compression · blog: new Minus Pad Extreme 2 and Minus Pad High Compression
- Thermal Grizzly — TG Putty · TG Putty datasheet
- Gelid — GP-Extreme · GP-Ultimate XL (product pages with FAQ) · GP-Ultimate press release (6 November 2019)
- Fujipoly — SARCON GR130A datasheet (ES_DS4130 v2.0, 21 February 2022)
- ARCTIC — TP-3 · TP-3 spec sheet
- ARCTIC — TP-3 manual
- ARCTIC — FAQ: What should you watch out for when using the thermal pads?
- ARCTIC — FAQ: What heat-conducting materials do we offer and how do they differ?
- Thermalright — Odyssey thermal pad · Odyssey II thermal pad
Liquid metal
- Thermal Grizzly — Conductonaut · Conductonaut datasheet
- Thermal Grizzly — Conductonaut safety data sheet (rev. 1.06, 4 July 2024)
- Thermal Grizzly — Conductonaut Quick Guide
- Thermal Grizzly — Conductonaut Extreme · datasheet · safety data sheet
- Thermalright — Silver King 1g · Silver King 3g
- Indium Corporation — Gallium-Based Liquid Metal Alloys as TIMs (PDS 97826 R11) · Liquid Metal Handout (99892 R1)
Device and chip makers
- Intel — How to Apply Thermal Paste
- Intel — Support article 000099579 (liquid metal on Intel processors)
- PlayStation Blog — PlayStation 5 Pro teardown: an inside look at the most advanced PlayStation console to date (21 April 2025)
- ASUS ROG — Patented process brings exotic liquid metal thermal compound to new ROG gaming laptops (2 April 2020)
- ASUS ROG — Celebrating five years of liquid metal in ROG laptops (17 January 2023, updated)
- ASUS ROG — ROG Astral GeForce RTX 5080 (product page)
- MSI — Advanced Technologies (MSI laptops)
- Lenovo — Legion Pro 7 (Intel) Liquid Metal Removal & Application SOP (service procedure, February 2023)
Research
- Viswanath R. et al. (2000). Thermal Performance Challenges from Silicon to Systems. Intel Technology Journal, Q3 2000 (vol. 4, issue 3).
- Hugo, Hoagland (1998). Scripta Materialia 38(3), DOI 10.1016/S1359-6462(97)00464-8 — OSTI record 603894 (liquid gallium in aluminium grain boundaries).
- Cai et al. (2025). Materials 18(5):1026 — doi:10.3390/ma18051026 (gallium embrittlement of aluminium).
- Liu et al. (2018), review. Materials 11(8):1384 — doi:10.3390/ma11081384 (gallium-based liquid metals and their reactions with other metals).
- Kim et al. (2023). Materials 16(18):6186 — doi:10.3390/ma16186186 (gallium, copper and nickel diffusion barriers).
- Wu, Kantharaj, Alsaati, Marconnet, Handwerker (2022). Investigation of thermal properties and thermal reliability of Ga-based low melting temperature alloys as thermal interface materials (TIMs). TMS 2022, Purdue University.
Is your laptop or console running hot or loud? Bring it to Silent Cloud TECH in Limassol for cleaning and maintenance of the cooling system — from €80, with the paste replaced by PTM7950 included in the price. Laptops can also come by ACS courier from anywhere in Cyprus, with return shipping on us. Diagnostics are €40, followed by a fixed quote before any work begins. See our services.
Call +357 25 030 676 or +357 94 044 066, message us on WhatsApp, or find us on Telegram at @SilentCloud_Tech. English and Russian spoken.